What should I do if UV resin/coating exhibits gelation? And what are the precautions to take?
Release time:
2014-06-24 13:38
In the coatings industry, it’s common for some customers to report gelation issues with UV resins or UV coatings. There are multiple factors that can cause UV resin gelation, and when troubleshooting this problem, it’s important to systematically rule out each potential cause one by one. So, what should you do if your UV resin or UV coating experiences gelation? What precautions should you take? Let’s take a closer look at the causes of gelation below.
Gelation refers to the phenomenon in which a resin or coating becomes thickened or clumped under specified temperature and time conditions. The main causes of gelation in resins or coatings include the following:
1. Due to the expiration date, the product has exceeded its shelf life. Under proper storage conditions, UV resin’s shelf life should not exceed six months, and it is best to use it within three months.
2. Storage issues—improper container selection. UV resin should be stored in plastic drums or metal drums with an inner plastic coating, as metal ions can lower the activation energy of the double bonds in UV resin, thereby triggering polymerization and causing the resin to gel. Therefore, if the plastic coating inside a plated drum is damaged and the metal layer is exposed, the resin will gel.
3. Storage conditions: Temperature too low. Storage temperatures that are too low (below 0℃) can cause the polymerization inhibitor in the paint film to precipitate out, leading to self-polymerization of the resin and resulting in resin gelation.
4. Storage Conditions: Avoid Direct Sunlight. During storage, UV resin must be strictly protected from direct sunlight; otherwise, it can easily undergo gelation.
5. If the buckets are filled too full, there won't be enough oxygen to inhibit polymerization, which can lead to resin gelation. Therefore, some space should be left to allow oxygen to inhibit polymerization effectively.
There are many factors that can cause UV coatings to gel, and the issue is not solely related to the resin itself. First, one should investigate whether improper storage conditions are the culprit. Since UV coatings contain photoinitiators, their storage requirements are somewhat more stringent than those for UV resins. They must be stored in a dark environment, completely shielded from light. Additionally, if the quality of the photoinitiator used is poor, even when stored in darkness, it may gradually decompose, leading to the gelling and hardening of the coating.
Precautions regarding gelation:
Monomer quality. The quality of the monomer is also an important factor affecting storage stability.
If the viscosity is too high, it may be mistakenly thought that the resin has gelated. Resins without added diluent monomers tend to have very high viscosity; some users might mistakenly believe that the resin has already gelated. In fact, a simple heating test can easily determine whether the resin has gelated or not. A resin that hasn't gelated will exhibit excellent fluidity when heated.
Regarding issues related to the use of UV resins, the methods and indicators for testing UV coating films are similar to those used for other coatings; however, they may vary depending on the specific application. Various problems can arise during the application of UV coatings. Among these, gelation during storage is closely linked to the UV resin itself, whereas other issues can generally be addressed by adjusting the formulation of the UV coating. Since UV coatings consist of a variety of components and are also influenced by factors such as the distance from the light source and the duration of illumination, the performance of the coating film is the result of the combined effects of these various factors. Even with the same formulation, if a different brand of resin is substituted—even if it’s the same type of resin—differences among resins from different manufacturers can alter the coating’s performance, necessitating adjustments to the formulation. However, as long as the resin has not undergone gelation or gelation has not occurred in the prepared coating mixture, the coating’s performance can be fine-tuned by modifying the formulation.
Share to:
Related News
Synthesis and Properties of Polyurethane Acrylate (PUA)
Polyurethane acrylate (PUA) is an important material characterized by excellent surface gloss, hardness, adhesion, and flexibility, as well as outstanding resistance to yellowing. Its wide range of applications gives it promising market prospects and significant development potential.
Introduction to Epoxy Acrylate
Epoxycrylates (EA) are a class of prepolymers widely used in the UV-curing field. The following provides an introduction to several commonly used epoxycrylates (EA) in the UV-curing domain, covering their structure, properties, and applications.
Performance Testing and Evaluation of UV Coating Cured Films
Testing and evaluating the performance of UV-coating cured films is one of the crucial steps in the production process of UV coatings. Conducting these tests and evaluations on the cured films helps ensure the stability of the coating’s quality and performance.