Tel
Tel
+8618142863185
Follow us
Official Accounts
Official Accounts
- Top
How to Improve the Weather Resistance of UV Topcoats
Release time:
2014-06-06 17:17
How to Improve the Weather Resistance of UV Topcoats
For outdoor UV topcoats, weather resistance is crucial; therefore, how to enhance the weather resistance of coatings is a very obvious question. So, how can we improve the weather resistance of UV topcoats?
I. Selection of Resin
To enhance weather resistance in outdoor UV topcoats, it is essential to select resins that exhibit excellent yellowing resistance, maintain stable film modulus under varying environmental conditions, possess high hardness, good flexibility, and superior scratch resistance. Among these requirements, the most suitable UV resin is a polyurethane resin based on multifunctional aliphatic acrylates. To reduce costs, it is also acceptable to appropriately blend a portion of modified epoxy acrylate resin with aliphatic polyurethane acrylates or pure acrylic resins.
II. Selection of Monomers
There is a contradiction in the use of monomers: From the perspective of skin irritation, alkoxylated acrylate monomers should be chosen; however, from the standpoint of weather resistance, alkoxylated acrylate monomers should not be selected. For weather-resistant topcoats, it is best to choose monomers such as TMPTA, HDDA, and TPGDA, as these can help reduce photodegradation.
III. Selection of Photoinitiators
Hydrogen-transfer-type photoinitiators have a relatively high yellowing coefficient; therefore, it is generally advisable to choose cleavage-type photoinitiators to help mitigate yellowing. Commonly used options in clear coats or colored systems include 1173, 184, and TPO.
IV. Selection of Other Additives
1. UV absorber
In other types of coatings, to enhance weather resistance, UV absorbers are often used to reduce the polymer’s UV absorption, or simple triplet-state quenchers are added to scavenge free radicals. However, in UV-curable coatings, maximum absorption of ultraviolet light is required during curing to generate more free radicals. If UV absorbers are added, they may partially shield the photoinitiator in the system, thereby slowing down the curing rate and reducing the polymer conversion rate. Experimental studies have shown that the optimal addition level is less than 0.1%, and among the additives, formamides perform better than benzotriazoles and aromatic ester compounds.
2. Hindered Amine Light Stabilizers (HALS) and Antioxidants
The primary feature of HALS is its photooxidation process, which generates nitroxyl radicals (R2NO·). These R2NO· radicals terminate the reaction by undergoing disproportionation or coupling reactions with free radicals on the polymer, yielding hydroxylamines and ether-hydroxylamines and ethers, respectively. These compounds then decompose into hydroperoxides, which in turn generate more R2NO· radicals. This cycle repeats continuously, significantly reducing the likelihood of resin degradation. Some experts believe that adding HALS can enhance the weather resistance of UV coatings.
Following the same principle as UV absorbers, the addition of HALS can also interfere with the free-radical reactions occurring during UV curing. When added at concentrations ranging from 0.1% to 0.05%, in matte coating systems (with gloss measured at 60° and less than 50), the surface may exhibit a persistent inability to dry. Therefore, it is recommended against adding HALS.
Antioxidants are divided into preventive antioxidants and chain-breaking antioxidants. Since they primarily function through redox reactions to inhibit the formation of peroxides, they have relatively little impact on UV curing and can therefore be selected as appropriate.
3. Selection of Certain Transparent Dyes
Dark or solid-color coatings still pose a challenge for UV coatings; however, in thin coatings, adding less than 3% of a transparent dye can enhance the shielding effect against UVA light in natural daylight—particularly the absorption or reflection of ultraviolet light in the 330–400 nm range found in sunlight—thereby reducing the coating’s susceptibility to photoaging.
4. Selection of fluorescent whitening agents
Fluorescent whitening agents absorb ultraviolet light and emit blue or violet light, thereby "complementing the blue light" in the coating to neutralize the yellow tint. After using fluorescent whitening agents, there is a competition between the whitening agents and the photoinitiators for light absorption; therefore, it is essential to select photoinitiators with higher initiation efficiency.
Share to:
Related News
Low Surface Energy Monomer Photocuring Applications
With the development of modern industry, light-curing technology is being increasingly widely applied across various fields—especially in printing, coatings, and plastics, where its role has become indispensable. Among these applications, low-surface-energy monomer-based light-curing technology stands out as a particularly important technique with extremely promising prospects.
Applications of Visible-Light Initiators
Visible-light initiators are a class of compounds capable of absorbing visible light and releasing free radicals or ions. They are widely used in fields such as UV-curable coatings, inks, and adhesives. In the application of visible-light initiators, they can accelerate the progression of photocuring reactions, thereby enhancing both the production efficiency and quality of the final products.
How to efficiently select oligomers (resins) in UV coating formulations
In UV coating formulations, the selection of oligomers (resins) is critically important, as they significantly influence both the performance and cost of the coating. To efficiently choose oligomers, it’s essential to consider multiple factors, such as molecular weight, chemical structure, viscosity, and surface tension. Below are some recommendations to help you select oligomers more effectively.