PCB Manufacturing Process and Overview of PCB Ink Composition
Release time:
2016-06-14 08:58
I. What is a PCB?
A PCB (Printed Circuit Board), known in Chinese as a printed circuit board or printed wiring board, is an essential electronic component. Because it is manufactured using electronic printing technology, it is referred to as a “printed” circuit board.


II. Types of PCBs
1. By substrate type
(1) Paper-based copper foil substrate;
(2) Composite substrate;
(3) Glass-fiber copper-clad laminate.
2. Classified by hardness and softness
(1) Rigid printed circuit boards (accounting for 85%);
(2) Flexible printed circuit boards (accounting for 15%).
3. By structure
(1) Single-sided board;
(2) Double-sided board;
(3) Multilayer board.
a. Single-sided board:

Advantages: Low cost; no need to drill holes;
Disadvantages: Wiring can only be done on one side, making the design more challenging than that of a multilayer board with double-sided boards.
b. Double-sided board:

Features: The circuit is complex but wiring is easy; drilling is required.
c. Multilayer board:

Features: Complex structure, multi-layer lamination, and perforation.
III. PCB Manufacturing Process
1. Substrate cutting, edge grinding, and cleaning


2. Circuit printing (resist ink)
Method 1 (UV method):

Method 2 (Exposure Method):

3. Line Etching
Method 1 (Etching Solution):

Etching: hydrochloric acid + etchant; Film removal: 3-5% NaOH
Method 2 (Alkaline Removal):
Alkali stripping solution: 1% NaCO3 solution
4. Solder mask, insulation, text

5. Stamping and forming

6. Computer detection

Overall Flowchart of PCB Formation

4. PCB Ink
PCB Ink Classification:

Basic composition of PCB ink:

1. Base resin
(1) Main resin for etch-resistant ink
Due to the chemical structural reaction of the ink during development:

Typically, the main resin in etch-resistant ink contains a large number of double bonds and also includes -COOH groups, with an acid value as high as 100–200 mg KOH/g or more.
The main resin designs for etch-resistant inks generally include the following types:
a. Copolymer of unsaturated acids (anhydrides) and unsaturated monomers;
b. Monomers or resins containing hydroxyl groups react with unsaturated anhydrides or resins containing anhydride groups;
c. Monomers or resins containing epoxy groups first react with acrylic acid, and then react with unsaturated anhydrides or resins containing anhydride groups;
d. Maleic anhydride-modified resin.
(2) Main resin of solder mask ink
Solder mask ink features: High temperature resistance—remains unchanged in color, does not carbonize, and does not crack after being subjected to temperatures above 260°C; high gloss.
Typically, the main resin types are as follows:
a. Epoxy resins—such as phenol-based epoxy and o-cresol-based epoxy;
b. Modified epoxy resins—acid anhydride-modified phenolic epoxy acrylate resin, hydroxylated bisphenol A epoxy open acid anhydride;
c. Modified acrylic resin—copolymer of styrene-anhydride-acrylic monomers with hydroxyl-containing acrylic monomers;
d. Modified melamine formaldehyde resin.
2. Filler
Common fillers: talc, kaolin, silica powder, fumed silica, barium sulfate, and others.
Conductive fillers: silver paste, copper paste, carbon black, etc.
Function: (1) Enhance the ink’s heat resistance and hardness;
(2) Enhance the adhesion between the ink and the substrate surface;
(3) Enhance the adhesion between ink and metal.
3. Colorant
Function:
(1) Identification, recognition
(2) Solder mask ink serves as the outer coating for PCBs. By using colorants of different hues, the product’s appearance can be enhanced, thereby increasing its added value.

4. Solvent
The organic solvent content in PCB ink typically ranges from 10% to 15%, serving to adjust the ink's viscosity.
High-boiling-point, environmentally friendly: DBE, DCAC, xylene, diethylene glycol dimethyl ether, and others;
The amount of organic solvents added to ink must be strictly controlled: too much can lead to prolonged baking times and poor adhesion, while too little can result in excessively high ink viscosity, making printing operations difficult.
V. Precautions
1. Ink thickness:
(1) Standard ink thickness: 10–25 microns (ink on the circuit surface, measured after curing);
(2) Ink thickness is too thin (less than 10 microns): This reduces heat resistance, acid and alkali resistance, and pencil hardness, making the ink prone to flaking.
(3) Ink thickness is too high (over 25 microns):
a. Lateral etching and enlargement;
b. The solvent is difficult to evaporate during the pre-baking process, which easily leads to adhesion of the exposed film and the formation of imprints on the film after exposure.
c. Reduced heat resistance, acid and alkali resistance, and gold-plating resistance.
2. Exposure amount
(1) The exposure amount needs to be adjusted according to the ink thickness:
a. Thick ink—high exposure amount;
b. Thin ink—low exposure.
(2) If the exposure energy is insufficient:
a. Lateral etching and enlargement;
b. Ink flaking;
c. After development, the ink surface turns white.
3. Pre-baking
(1) If pre-baking is insufficient, the following situations will occur:
If the ink surface is not sufficiently dry, it may stick to the exposure negative during exposure, or the ink surface may show exposure marks.
During development, the ink is easily eroded by the developer solution, causing lateral etching to expand and making the ink prone to flaking. In severe cases, this can even lead to whitening of the ink surface.
(2) If pre-baking is excessive, the following situations will occur:
Thermosetting resins will initiate a chemical crosslinking reaction, leading to issues such as incomplete development and inability to develop. 
Share to:
Related News
Pad printing is one of the special printing techniques. It enables the printing of text, graphics, and images onto surfaces of irregularly shaped objects and is now becoming an important specialized printing method. For example, the text and patterns on mobile phone surfaces are printed using this technique. Similarly, surface printing on computer keyboards, instruments, meters, and many other electronic products is also commonly carried out via pad printing. Pad printing technology is a relatively newer printing process compared to screen printing. As silicone rubber pad printing heads began to emerge, this technology gradually developed and improved. Silicone rubber pad printing heads can easily separate from various types of materials—including inks. By using these heads as printing stamps, it’s possible to print simultaneously on both concave and convex surfaces, inclined surfaces, and even vertical surfaces.
Water transfer printing is a printing technique that uses water pressure to hydrolyze polymers, transferring color-patterned transfer papers or plastic films onto surfaces. As consumer demands for product packaging and decoration continue to rise, the applications of water transfer printing are becoming increasingly widespread. Its indirect printing principle and impeccable printing results effectively address many challenges in surface decoration of various products, and it is primarily used for transferring designs onto ceramics, glass decals, and similar materials.
Those crafts that are both familiar and unfamiliar to us: hot stamping.
Gilding, also known as hot stamping, is a printing and decorative technique. A metal printing plate is heated, and foil is pressed onto the printed material to emboss gold-colored text or patterns. This process relies on the principle of thermal transfer, in which the aluminum layer from electroplated aluminum foil is transferred onto the surface of the substrate to create a distinctive metallic effect. Since the primary material used in gilding is electroplated aluminum foil, gilding is also referred to as electroplated aluminum hot stamping.