Analysis of Common Issues with UV PCB Ink (Part 3)
Release time:
2025-03-20 08:59
During the PCB manufacturing process, especially after the exposure or baking steps, ink often overflows from the vias, resulting in via blockage or via bursting. This not only severely affects the visual quality of the PCB but can also degrade the electrical connection performance and stability of the circuit, thereby compromising the overall reliability and service life of the product. Via blockage and via bursting can lead to short circuits, open circuits, or unstable signal transmission, profoundly impacting the performance and reliability of the entire electronic device.
The main reasons are as follows:
I. Exposure Issues
1. Poor degassing action during exposure: During exposure, the air trapped between the film and the work plate fails to be completely expelled. This may be due to insufficient precision of the exposure equipment or inadequate maintenance, resulting in poor adhesion and subsequently affecting the exposure quality, causing ink to overflow into the holes.
2. Poor vacuuming during exposure: Insufficient vacuuming during exposure, poor sealing of the vacuum system, or inadequate vacuuming time can lead to air bubbles forming between the film and the work plate, thereby affecting the exposure quality and causing ink overflow.
3. Unstable vacuum pressure: Fluctuations in vacuum pressure during exposure may be caused by a faulty pressure sensor or an unstable control system, which can affect the adhesion between the film and the work plate, thereby compromising the uniformity of exposure and leading to ink overflow.
II. Positioning Issues
1. The positioning sheet was not inserted into the hole: The positioning sheet was either not properly inserted into the hole, or its size and shape did not match those of the hole, causing displacement between the film and the work plate during exposure and resulting in ink overflowing from the hole.
2. Inaccurate positioning: Even if the positioning sheet is inserted, inaccurate positioning can still cause ink to overflow from the holes during printing. This may be due to insufficient precision in the positioning system or improper maintenance.
III. Baking Issues
1. Non-segmented temperature ramp-up during post-baking: During the post-baking process, there was no segmented temperature ramp-up, or the temperature control of the baking equipment was inaccurate, and the sensors were malfunctioning, resulting in uneven ink curing. Consequently, in some areas, the ink did not fully cure and overflowed.
2. Improper setting of segmented temperature control: If the temperature in the low-temperature segment is too high, the ink will begin to cure prematurely in this segment, leading to ink overflow in the subsequent high-temperature segment. Conversely, if the duration of the low-temperature segment is insufficient, the ink will not fully cure during this phase and will continue to cure—and eventually overflow—when it enters the high-temperature segment. Additionally, if the temperature in the high-temperature segment is too low or the duration is excessively long, it may result in incomplete curing or over-curing of the ink.
3. Uneven temperature distribution in the oven: The temperature inside the oven is unevenly distributed, possibly due to aging or damage of the oven’s heating elements, resulting in uneven heating of the ink. In some areas, the ink overheats and spills over.
4. The direction of hot air is unstable: The inconsistent direction of hot air inside the oven may be due to a malfunction or improper maintenance of the hot-air circulation system, which affects the uniform heating and curing of the ink.
IV. Tin Spraying Issues
1. Failure to pre-bake and heat before soldering: Before soldering, the PCB was not pre-baked and heated, or the temperature and duration of the pre-baking and heating were improperly set, resulting in uneven heating of the ink during soldering and causing it to overflow.
2. Excessive soldering temperature: If the soldering temperature is too high, or if the temperature control of the soldering equipment is inaccurate, or if the sensor malfunctions, the ink may expand and overflow at high temperatures.
V. Film Design Issues
1. Poor film design: The film design is unreasonable, with hole positions not matching the circuit paths, or with line widths and spacings that are improperly designed, causing ink to easily overflow from the holes during the printing process.
2. Foreign Matter on Film Surface: Dust, fibers, and other foreign matter adhering to the film surface, or contamination or damage to the film during production or storage, can affect exposure quality and cause ink bleeding.
VI. Conclusion
The phenomena of solder mask overflow from holes during PCB manufacturing—resulting in blocked vias and popped vias—are rooted in complex and diverse factors. To effectively control and reduce the occurrence of these issues, manufacturers need to take a multi-faceted approach, ensuring that every stage of the process achieves high precision and stability. Through continuous process improvements and technological innovations, manufacturers can enhance the aesthetic quality and circuit performance of PCBs, thereby boosting the overall reliability and service life of electronic products.
Disclaimer: The above content is sourced from the internet and is for reference only. If any infringement occurs, please contact us, and we will remove it promptly.
Share to:
Related News
Analysis of Common Issues with UV PCB Ink (Part 2)
In the manufacturing process of PCBs (printed circuit boards), a particularly critical issue is the separation of ink from the copper surface in areas where the ink is supposed to completely cover large copper surfaces, resulting in voids. This problem severely affects the electrical connectivity performance and product reliability of PCBs, and it also impacts the aesthetic quality of the PCBs. The formation of voids can not only lead to poor electrical conductivity but may also reduce the durability and stability of the PCB.
Analysis of Common Issues with UV PCB Ink (Part 1)
In the manufacturing process of PCBs (printed circuit boards), uneven UV PCB ink application is a common and serious issue. Specifically, the ink fails to adhere uniformly across the board surface, resulting in localized spots, streaks, or patches of white ink. In severe cases, this can even prevent the ink from being applied altogether. This phenomenon not only severely affects the visual quality of the PCB but also poses a potential threat to the electrical connectivity and stability of the circuit.
Detailed Explanation of Key Factors in Selecting UV PCB Ink Formulations (Part 2)
In the formulation design of UV PCB inks, in addition to pigments, binders, and photopolymerization initiators, the selection of curing agents, solvents, and additives, as well as the compatibility with the substrate material, are also crucial aspects that cannot be overlooked. The choice and combination of these components directly affect the ink’s curing speed, printing performance, and adhesion and durability on various substrates.