Causes of Common Issues in UV Vacuum Plating (Part 4)


In the UV vacuum plating process, the appearance and quality of the plating layer are crucial indicators for evaluating the coating performance. However, in practical operations, various coating defects frequently arise, among which the phenomena of "undercutting" and "orange peel" stand out particularly. These phenomena not only compromise the aesthetic appeal of the product but can also adversely affect its performance and service life. Therefore, a thorough analysis of the causes behind undercutting and orange peel is of great significance for improving plating quality and optimizing the process.

I. Underbite Phenomenon

1. Line speed too slow:

(1) The excessively slow line speed causes the primer to absorb too much heat during the curing process, thereby accelerating the drying of the primer.

(2) Untimely adjustment of the production line: The line speed was not adjusted promptly based on factors such as coating thickness and material.

2. The substrate surface is uneven:

(1) Poor quality of base material or inadequate injection molding process can result in defects on the substrate surface, thereby affecting the adhesion of the coating.

(2) Poor quality of base material: The raw materials themselves have defects, such as pores and cracks.

(3) Poor injection molding process: Improper control of parameters such as temperature and pressure during injection molding results in an uneven substrate surface.

3. The solvent has excessively strong dissolving power:

(1) Improper solvent selection: If the solvent has excessively strong dissolving power, it may cause the primer to be dissolved by the topcoat, resulting in a phenomenon known as "primer bite."

(2) Coating formulation issue: The solvent in the coating is incompatible with the primer.

II. Orange Peel Effect

1. Substrate contamination:

(1) Inadequate substrate cleaning: The substrate surface contains contaminants such as oils and dust, which impair the leveling property of the coating.

(2) Poor storage conditions for the substrate: The storage environment contains contaminants such as dust and oil stains.

2. Poor paint leveling:

(1) Coating formulation issues: Insufficient or inappropriate leveling agents in the coating can result in an uneven coating surface.

(2) Improper paint storage: The paint deteriorates during storage, leading to a decline in its leveling performance.

3. Improper spraying pressure:

(1) Spraying equipment issues: Unstable or improperly adjusted spraying equipment pressure can cause the coating surface to develop a wavy appearance.

(2) Improper spraying operation: The spraying pressure was not maintained at a stable level during the spraying process.

4. Insufficient IR temperature and leveling time:

(1) Improper IR baking temperature settings: If the temperature is too low or the leveling time is insufficient, the coating will fail to level completely.

(2) Too-short leveling time: Insufficient leveling time prevents the coating from fully leveling out.

5. The primer has too high a viscosity:

(1) Primer formulation issue: Improper use of viscosity modifiers in the primer affects the leveling properties of the coating.

(2) Improper storage of primer: The primer deteriorates during storage, leading to an increase in viscosity.

6. Coating too thin:

(1) Insufficient coating application: During the spraying process, the amount of paint applied is insufficient, making it impossible to form a uniform coating.

(2) Excessive spray distance: An excessively long spray distance results in uneven coating application.

III. Summary

In summary, the causes of bottom-biting and orange-peel defects in UV vacuum plating processes are complex and multifaceted, involving factors such as line-speed control, substrate quality, solvent selection, coating formulation, spraying equipment, operational skills, as well as baking temperature and duration. To effectively prevent and address these issues, manufacturers must take a holistic approach from the very beginning: rigorously control raw material quality, optimize injection-molding processes, carefully select solvents and coating formulations, regularly maintain and calibrate spraying equipment to ensure stable spray pressure and appropriate spray distance. At the same time, they should promptly adjust production-line speed according to coating thickness and material characteristics, and properly set baking temperature and leveling time. By adopting a comprehensive strategy, continuously optimizing production processes, and strengthening quality monitoring and inspection throughout the plating process, potential problems can be identified and resolved in a timely manner. Only in this way can we continually enhance plating quality and product market competitiveness, providing customers with higher-quality, more aesthetically pleasing coated products.

Disclaimer: The above content is sourced from the internet and is for reference only. If any infringement occurs, please contact us, and we will remove it promptly. 

Share to:

Related News


Causes of Common Issues in UV Vacuum Plating (Part 3)

In UV vacuum plating technology, ensuring plating quality is a critical step. However, during actual operations, a series of issues often arise that affect both the appearance and performance of the plating. Among these, shrinkage pits and whitening/fogging phenomena are particularly common and challenging to address. Shrinkage pits typically manifest as depressions or holes on the surface, which not only detract from the product’s aesthetic appeal but may also compromise the protective performance of the plating layer. Meanwhile, the whitening/fogging phenomenon causes the plated surface to appear unevenly white or hazy, similarly having a detrimental impact on the overall product quality.


Causes of Common Issues in UV Vacuum Plating (Part 2)

The UV vacuum plating process has gained a prominent position in surface treatment for various products thanks to its distinctive luster and excellent corrosion resistance. However, in actual production, surface defects often pose significant challenges for manufacturers, affecting the overall product quality and customer satisfaction. Defects such as pinholes, particles, and iridescence not only detract from the aesthetic appeal of the products but can also compromise their functional performance and durability. A thorough investigation into the causes of these defects is crucial for enhancing the quality of products produced using the UV vacuum plating process.


Causes of Common Issues in UV Vacuum Plating (Part 1)

In modern industrial manufacturing, the UV vacuum plating process—thanks to its high efficiency, environmental friendliness, and excellent decorative performance—is widely used in various fields such as automotive, electronics, and furniture. However, in actual production, poor adhesion and inadequate curing have become key factors that hinder the improvement of this process’s quality. Conducting an in-depth analysis of the specific causes behind poor adhesion and inadequate curing, and proposing effective countermeasures to address these issues, is of great significance for enhancing both the product quality and production efficiency of the UV vacuum plating process.