Operating Procedures for Applying Three-Proof Coating (Part 2)


The dip-coating method involves completely immersing workpieces such as circuit boards into a conformal coating liquid. Relying on the surface tension and adhesion properties of the coating liquid, this process forms a uniform protective film on the surface of the workpiece. It is particularly suitable for mass production of small, simply structured electronic components or circuit boards that demand high coating uniformity. Thanks to its advantages—such as high production efficiency and excellent coating uniformity—the dip-coating method has become an important choice in large-scale circuit-board protection manufacturing. However, the dip-coating process involves numerous complex factors. From the precise placement and removal of PCBs to the meticulous control of parameters like dipping speed, dipping time, and lifting speed, every step directly affects the final quality of the coating film and its protective performance. Even a slight oversight can lead to defects such as uneven coating thickness, air bubbles, or dripping, seriously compromising the circuit board’s protective capabilities.

The following are the detailed specifications for dip coating operations:

I. PCB Placement and Removal

Place the PCB smoothly onto the fixture of the dip-coating equipment, ensuring that the PCB is immersed vertically into the coating liquid and avoiding any tilting that could lead to uneven coating thickness. After dipping is complete, carefully and uniformly remove the PCB from the coating liquid at a slow pace to prevent vigorous agitation of the liquid, which could cause bubble formation.

II. Pre-impregnation

For substrates with high absorbency, a pre-soaking treatment can be performed before the formal dip-coating process. Specifically, the circuit board is briefly immersed in a low-concentration conformal coating or a dedicated pre-soaking solution to reduce uneven absorption of the coating liquid during the formal dip-coating. The typical pre-soaking time is 5 to 10 seconds.

3. Formal Dip Coating

Slowly immerse the fixture holding the circuit board into the coating liquid until the circuit board is completely covered. The immersion speed should be moderate to avoid bubble formation. Keep the circuit board immersed in the coating liquid for a sufficient period of time to ensure that the coating liquid thoroughly wets the surface of the circuit board.

4. Dipping Speed

The dip-coating speed should be adjusted according to the viscosity of the conformal coating and the size and shape of the PCB. Generally, the dip-coating speed is controlled within the range of 1–5 cm/s. If the speed is too fast, the coating film may not have enough time to adhere evenly to the PCB surface, resulting in uneven thickness. Conversely, if the speed is too slow, the coating film will become excessively thick, increasing costs and potentially affecting product performance. For small PCBs, the dip-coating speed can be slightly increased; for large or complex-structured PCBs, the dip-coating speed should be slowed down to ensure coating quality.

V. Dipping Time

The immersion coating time typically ranges from 1 to 5 seconds, with the specific duration depending on the type and viscosity of the conformal coating, the desired film thickness, and the complexity of the circuit board. If the immersion time is too short, the coating film will be insufficiently thick, resulting in poor protective performance. Conversely, if the immersion time is too long, the coating film will become excessively thick, making it prone to issues such as sagging and bubble formation. The optimal immersion coating time can be determined through experimentation.

6. Increase speed

The speed at which the PCB is lifted from the dip-coating tank also affects the quality of the coating film. The lifting speed should be uniform and stable, typically maintained within the range of 1–3 cm/s. If the lifting speed is too fast, the coating film surface may develop flow marks and bubbles; if the lifting speed is too slow, the coating film may drip during the lifting process, leading to waste and contamination.

7. Present and drain

After soaking is complete, use the lifting device to gently and slowly raise the circuit board out of the coating solution. During the extraction process, maintain a vertical position to prevent tilting, which could cause uneven distribution of the coating solution on the circuit board surface. Once extracted, hang the circuit board on a draining rack to allow any excess coating solution to drip off naturally; the typical draining time is 1 to 3 minutes.

VIII. Summary

Coating the conformal coating via dip-coating is a meticulous and rigorous process. Each step is like a critical component in a precision instrument—interconnected and mutually influential—collectively determining the quality of the final coating film and the effectiveness of circuit board protection. From the careful, smooth vertical placement and removal of PCBs to the painstaking treatment of special substrates during the pre-dipping stage; from the precise control of speed and duration during the actual dip-coating process to the stringent monitoring of speed stability throughout the curing phase; and right through to the meticulous attention paid to details during the transfer and draining stages—every single step demands unwavering vigilance and precision.

Disclaimer: The above content is sourced from the internet and is for reference only. If any infringement occurs, please contact us, and we will remove it promptly. 

Share to:

Related News


Operating Procedures for Applying Three-Proof Coating (Part 1)

Among the many methods for applying conformal coatings, the brush-coating method is widely used—particularly in small-batch production, localized coating applications, and scenarios that demand high coating precision—thanks to its flexible operation and versatility across various application environments. However, despite its seemingly simple nature, the brush-coating method actually has stringent requirements for operational standards. Every single detail can affect the final coating result and, consequently, the protective performance of the circuit board.


Introduction to the Three-Proof Coating Process (Part 3)

Three-proof coatings, also known as three-proof paints or electrical protective adhesives, are specialized coating materials that offer protection against moisture, dust, mold, and electrical insulation. By being applied to the surface of electronic device circuit boards, these coatings form a uniform and dense protective film, effectively shielding the circuit boards from environmental hazards. Among the various application techniques for three-proof coatings, spray coating has become one of the most widely used methods in the industry due to its high efficiency and even distribution characteristics.


Introduction to the Three-Proof Coating Process (Part 2)

As a specially formulated coating, conformal coating is widely used to protect printed circuit boards and related equipment from environmental degradation, thereby enhancing their service life and reliability. Among the many coating processes, the dip-coating method holds a prominent position in applications requiring complete coverage, thanks to its unique advantages.