The “traffic leader” in the light-curing resin industry


In the previous issue, we introduced that the resin used in the largest quantity in the light-curing industry is epoxy acrylate, and among epoxy acrylates, bisphenol A epoxy acrylate is the most commonly used and widely employed.

Bisphenol A epoxy acrylate is produced by reacting bisphenol A epoxy resin with acrylic acid. The bisphenol A epoxy resin itself is synthesized by reacting bisphenol A with epichlorohydrin under alkaline conditions. By carefully controlling the molar ratio of the two raw materials and the reaction conditions, bisphenol A epoxy resins with varying degrees of polymerization can be obtained. The higher the degree of polymerization, the greater the molecular weight and the lower the epoxy value.

As shown in the figure, in the general formula, n represents the degree of polymerization, and its value typically ranges from 0 to 25. Generally, low-molecular-weight epoxy resins have an average n value less than 2, with softening points below 50°C. Medium-molecular-weight epoxy resins have n values between 2 and 5, and their softening points fall within the range of 50°C to 95°C. Epoxy resins with n values greater than 5 are referred to as high-molecular-weight resins, with softening points exceeding 100°C. Commercially available bisphenol A epoxy resins can have n values ranging from 0 to 12. However, to obtain bisphenol A epoxy acrylates with high curing speeds, it is common practice to select bisphenol A epoxy resins that feature a high epoxy equivalent weight and low viscosity. This allows for the introduction of more acrylate groups. Therefore, in most cases, low-molecular-weight bisphenol A epoxy resin models with an approximate n value of 0 are preferred. For example, commonly used domestic grades include E-51 (epoxy value: 0.51 ± 0.03 eq/100g) and E-44 (epoxy value: 0.44 ± 0.03 eq/100g).

The ring-opening esterification of the epoxy groups in bisphenol A epoxy resin with acrylic acid, catalyzed by a catalyst, is an exothermic reaction. Typically, the epoxy resin is heated to around 80°C, after which a mixture of acrylic acid, catalyst, and polymerization inhibitor is added dropwise. Once the reaction has progressed substantially, the temperature is gradually raised to 100–120°C to ensure complete reaction. Samples are taken for acid value testing; once the acid value drops below the target level, the reaction mixture is cooled and discharged. Since bisphenol A epoxy acrylate exhibits high viscosity at low temperatures, 20% of a UV monomer (such as TPGDA or TMPTA) is usually added to dilute and reduce its viscosity, facilitating subsequent processing and use.

In the early stages of the bisphenol A epoxy acrylate reaction, catalysts are typically added to promote the reaction. Commonly used catalysts include tertiary amines and quaternary ammonium salts—for example, triethylamine, N,N-dimethylbenzylamine, trimethylbenzylammonium chloride, triphenylphosphine, triphenylantimony, acetylacetonate chromium, and tetraethylammonium bromide. Although triethylamine is inexpensive and readily available, its catalytic activity is relatively low, and the resulting product exhibits slightly poorer stability. Quaternary ammonium salts, while offering slightly higher catalytic activity, are somewhat more expensive. Triphenylphosphine, triphenylantimony, and acetylacetonate chromium exhibit high catalytic activity and produce products with low viscosity; however, their coloration tends to be darker.

Since bisphenol A epoxy acrylate has a relatively high reaction temperature, in order to prevent the polymerization of acrylic (esters) during heating, it is necessary to add a certain amount of polymerization inhibitor. Commonly used polymerization inhibitors include hydroquinone, methylhydroquinone, and p-methoxyphenol.

The above is the synthesis reaction process of bisphenol A epoxy acrylate.

Disclaimer: The above content is sourced from the internet and is for reference only. If any infringement occurs, please contact us, and we will remove it promptly. 

Share to:

Related News