Dimensional accuracy is one of the key factors determining the success of dental restorations. In UV‑based 3D printing, dimensional inaccuracies manifest as discrepancies between the printed part’s dimensions and the design specifications—resulting in restorations that are either oversized or undersized, or in models that exhibit shrinkage or expansion. Such deviations can compromise the restoration’s marginal fit and seating accuracy within the patient’s mouth. Exposure time, post‑curing procedures, and the storage duration of the printed parts are the primary factors influencing dimensional accuracy.
I. Dimensional Deviations Caused by Improper Exposure Time
Exposure time is a critical parameter that affects the dimensional accuracy of printed parts. As UV exposure time increases, the dimensions of the printed part can grow significantly—excessive exposure leads to over‑polymerization and volumetric expansion, causing the part to deviate from its intended design specifications.
Insufficient exposure time also poses significant problems. Incompletely cured resin exhibits inadequate strength and weak interlayer adhesion, which may lead to deformation of the model during post-processing or in clinical use. Precise control of exposure time is critical for the accurate clinical placement of dental restorations; excessive deviation can directly compromise marginal fit.
II. Dimensional Changes Caused by Post-Curing
Post‑curing is a post‑processing step in which the printed part is placed in a UV curing chamber for a second exposure, with the aim of further crosslinking the resin and enhancing its mechanical properties. However, the post‑curing process can also lead to dimensional changes.
The study found that post‑curing can induce a certain degree of dimensional deviation in surgical guides, attributable to additional shrinkage resulting from extra crosslinking during the polymerization process. Solvent cleaning can partially mitigate the dimensional effects of post‑curing.
III. Dimensional Drift Over Time in Printed Parts
The dimensions of photopolymer‑based printed models do not remain stable once printing is complete. Studies have shown that 3D‑printed resin models suffer from inadequate dimensional stability; as they are left to sit, they undergo shrinkage and deformation over time.
The positional offset of the implant analogues aligns with the model’s shrinkage direction. As storage time increases, both the three-dimensional deviation and angular deviation of the analogues increase significantly. Accordingly, it is recommended to fabricate the restorations as soon as possible after printing the model to prevent accuracy loss caused by prolonged storage.
IV. Conclusion
Dimensional accuracy deviations in dental UV‑based 3D printing stem from multiple stages. Insufficient exposure time leads to incomplete curing, while excessive exposure can cause over‑polymerization and volumetric expansion; post‑curing, additional crosslinking reactions may also introduce dimensional errors; and prolonged storage results in resin shrinkage, progressively degrading model accuracy. In practice, it is essential to calibrate exposure parameters according to the resin type, standardize the post‑curing protocol, and place the restoration within the prescribed time window. For implant models and surgical guides that demand high precision, controlling these factors is particularly critical.
Disclaimer: The above content has been compiled from publicly available sources and is provided for reference only. If any infringement occurs, please contact us, and we will address it promptly.
Bossin Related Product Recommendations – 3D Printing | ||
Dentistry | ||
Product Model/English Abbreviation | Product Name/Product Type | Product Features |
B-100M | Bisphenol A epoxy acrylate | Low viscosity, high hardness, high gloss, and high body. |
B-113 | Bisphenol A epoxy acrylate | High hardness, high gloss, high fullness, containing 20% TPGDA. |
B-276H | Aliphatic polyurethane acrylate | High hardness, fast curing, excellent toughness, and low yellowing. |
B-296 | Aliphatic polyurethane acrylate | Fast curing, chemical resistance, yellowing resistance, impact resistance |
B-296M | Polyurethane acrylate | Fast curing, resistant to polar solvents, yellowing-resistant, and impact-resistant. |
B-301 | Aromatic polyurethane acrylate | Fast curing, excellent toughness, and good sandability. |
B-302 | Aromatic polyurethane acrylate | Fast curing, high strength, excellent toughness, and good grindability. |
B-368 | Aliphatic polyurethane acrylate | Good toughness, excellent leveling, excellent bend resistance, and excellent heat resistance. |
B-376 | Aliphatic polyurethane acrylate | LED yellowing is minimal, and the nail polish formulation exhibits excellent stability. |
B-609 | Aliphatic polyurethane acrylate | Fast curing, high hardness, scratch resistance, and chemical resistance. |
B-79D | Polyester acrylate | High hardness, low yellowing, and high evaporation efficiency at elevated temperatures. |
Monomer Recommendation | ||
Product Model/English Abbreviation | Product Name/Product Type | Product Features |
BM1211 (HPMA) | Hydroxypropyl methacrylate | HEMA-free, high strength, low irritation, and excellent adhesion |
BM2223 (TPGDA) | Di(propylene glycol) diacrylate | Good flexibility and low volatility |
BM3231 (TMPTA) | Trimethylolpropane triacrylate | High crosslink density, high hardness, high gloss, and excellent wear resistance. |
BM3235 (PET3A) | Pentaerythritol triacrylate | Fast curing, high crosslink density, high hardness, and chemical resistance. |
BM3380 (3EO-TMPTA) | Pentaerythritol triacrylate | More flexible and less irritating than TMPTA. |